Material Notes:
Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is specially formulated with proprietary additive chemistry to meet the severe requirements of naturally aspirated and turbocharged, two-cycle, low- to medium speed gas engines. Hydroclear El Mar Ashless Supreme is particularly effective in engines and operating conditions which promote the formation of severe port carbon. Hydroclear El Mar Ashless Supreme has demonstrated successful performance results in severe duty engines manufactured by the following companies: Clark, Cooper Bessemer, Worthington (two-cycle)Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
Viscosity Measurement 135
135
Viscosity Index
Saybolt Viscosity at 100°F 567 SUS
567 SUS
Saybolt Viscosity at 210°F 77 SUS
77 SUS
Kinematic Viscosity at 40°C (104°F) 110 cSt
110 cSt
Kinematic Viscosity at 100°C (212°F) 14.5 cSt
14.5 cSt
Ash 0.030 %
0.030 %
Sulfated Ash
ASTM Color 1.5
1.5
Thermal Properties Metric English Comments
Pour Point -34.4 °C
-30.0 °F
Flash Point 221 °C
430 °F
Chemical Properties Metric English Comments
Total Acid Number 0.84
0.84
ASTM D974
Total Base Number 1.8
1.8
Descriptive Properties Value Comments
Carbon Residue 0.1 wt. %