ConocoPhillips Hydroclear® 68 2 EP gear Oil

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® 68 2 EP gear Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary additive chemistry and Conoco premium oils hydrocracked base oil. It is recommended for use in severe service enclosed-gear sets. Hydroclear EP Gear Oil provides “clean gear” performance with exceptional oxidation inhibition, EP load-carrying capacity, foam control, rust and corrosion protection and rapid low-temperature demulsibility. Hydroclear EP Gear Oil is capable of extending intervals between oil changes by providing “clean gear” performance, coupled with superior oxidation control. Hydroclear EP Gear Oil significantly exceeds the requirements of and has been formally approved by Cincinnati Milacron in accordance with its Lubricant Specifications (ISO 68 to 460, respectively – P-63, 76, 77, 74, 59 and 35). Hydroclear EP Gear Oil exceeds the latest AGMA Specification 9005 (replacement for 250.04) and U.S. Steel 224 Specification for enclosed-gear lubricants.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.874 g/cc
0.0316 lb/in³
Viscosity Measurement 98
98
Viscosity Index
Saybolt Viscosity at 100°F 374 SUS
374 SUS
Saybolt Viscosity at 210°F 56 SUS
56 SUS
Kinematic Viscosity at 40°C (104°F) 72 cSt
72 cSt
Kinematic Viscosity at 100°C (212°F) 8.7 cSt
8.7 cSt
ASTM Color 2.5
2.5
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
Four Ball Wear 0.300 mm
0.0118 in
Timken Test 31700 g
70.0 lb
Thermal Properties Metric English Comments
Pour Point -34.4 °C
-30.0 °F
Flash Point 235 °C
455 °F
Descriptive Properties Value Comments
Corrosion, Copper Strip 1B
Demulsibility, Emulsion 0
ASTM D2711
Demulsibility, Free Water 85
ASTM D2711
Demulsibility, Water in Oil 0.6
ASTM D2711
Emulsion Characteristics (40-40-0) 15 minutes
Foam Control (Sequence I,II,III) 0-0-0
FZG Pass 12 Load Stages
Oxidation Control 1.2 % vis. increase
ASTM D2893