Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical NBR 6830 High Acrylonitrile Polymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LG Chemical NBR 6830 High Acrylonitrile Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: NBR 6830 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6830 is a non staining, medium low mooney, and medium high acrylonitrile polymer designed for easy processing, high productivity and excellent elastic properties. NBR 6830 offers very low mold fouling, fast cure, and high resilience. NBR 6830 is low mooney version of NBR 6840Applications: NBR 6830 is recommended to use in wide range of general purpose applications including injection molded o-rings, calendared belting, extruded hose and sponge.CAS No: 9003-18-3Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Volatiles 0.30 %
0.30 %
Mooney Viscosity 31
<br>@Temperature 100 °C
31
<br>@Temperature 212 °F
ML 1+4
Ash <= 1.0 %
<= 1.0 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.0 MPa
<br>@Temperature 145 °C,<br> Time 2990 sec
3920 psi
<br>@Temperature 293 °F,<br> Time 0.830 hour
cured; ASTM D412
Elongation at Break 500 %
<br>@Temperature 145 °C,<br> Time 2990 sec
500 %
<br>@Temperature 293 °F,<br> Time 0.830 hour
cured; ASTM D412
300% Modulus 0.0142 GPa
<br>@Temperature 145 °C,<br> Time 2990 sec
2.06 ksi
<br>@Temperature 293 °F,<br> Time 0.830 hour
cured; ASTM D412
Descriptive Properties Value Comments
Bound AN Content 0.34
Color Light Tan
Components HAF (IRB#7)
40 phr, ASTM D3187
NBR 6830
100 phr, ASTM D3187
Stearic Acid
1 phr, ASTM D3187
Sulfur
1.5 phr, ASTM D3187
TBBS
0.7 phr, ASTM D3187
ZnO
3 phr, ASTM D3187
Copyright © lookpolymers.com All Rights Reserved