| Category | Ceramic |
| Manufacturer | Chosun Refractories |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Chosun Refractories GUN-140L Light-Weight Gunning Castable.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Rupture | 2.89e-7 - 0.00177 GPa <br>@Temperature 110 °C,<br> Time 86400 sec |
0.0000419 - 0.256 ksi <br>@Temperature 230 °F,<br> Time 24.0 hour |
|
| 0.000981 - 0.001962 GPa <br>@Temperature 1000 °C,<br> Time 10800 sec |
0.142 - 0.2846 ksi <br>@Temperature 1830 °F,<br> Time 3.00 hour |
||
| Compressive Strength | 1.96 - 4.41 MPa <br>@Temperature 1000 °C,<br> Time 10800 sec |
284 - 640 psi <br>@Temperature 1830 °F,<br> Time 3.00 hour |
Cold Crushing Strength |
| 4.90 - 6.86 MPa <br>@Temperature 110 °C,<br> Time 86400 sec |
711 - 996 psi <br>@Temperature 230 °F,<br> Time 24.0 hour |
Cold Crushing Strength |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.4653 W/m-K <br>@Temperature 260 °C |
3.224 BTU-in/hr-ft²-°F <br>@Temperature 500 °F |
|
| 0.48852 W/m-K <br>@Temperature 540 °C |
3.3849 BTU-in/hr-ft²-°F <br>@Temperature 1000 °F |
||
| 0.55831 W/m-K <br>@Temperature 800 °C |
3.8684 BTU-in/hr-ft²-°F <br>@Temperature 1470 °F |
||
| Maximum Service Temperature, Air | 1400 °C | 2550 °F | limited |
| Shrinkage | -0.400 % <br>@Temperature 1000 °C,<br> Time 10800 sec |
-0.400 % <br>@Temperature 1830 °F,<br> Time 3.00 hour |
|
| -0.150 % <br>@Temperature 110 °C,<br> Time 86400 sec |
-0.150 % <br>@Temperature 230 °F,<br> Time 24.0 hour |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 47 % | 47 % | |
| SiO2 | 32 % | 32 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Installation Method | Gynning | |
| Main Applications | Fireproof insulating Part | |
| Material Required for Estimating (kg/?) | 1,500 | |
| Water Required for Casting(%) | Nozzle Mixing |