Chicago Extruded Metals BioBrass® UNS C22600 Copper-Zinc Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Chicago Extruded Metals (CXM)
Trade Name BioBrass®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chicago Extruded Metals BioBrass® UNS C22600 Copper-Zinc Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.77 g/cc
0.317 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 70
70
Tensile Strength 276 - 669 MPa
40000 - 97000 psi
Tensile Strength, Yield 75.8 - 427 MPa
11000 - 62000 psi
Elongation at Break 3.0 - 45 %
3.0 - 45 %
Machinability 30 %
30 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 173 W/m-K
1200 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 86 - 89 %
86 - 89 %
Iron, Fe 0.050 %
0.050 %
Lead, Pb 0.050 %
0.050 %
Other, total 0.20 %
0.20 %
Zinc, Zn 10.7 - 13.7 %
10.7 - 13.7 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000431 ohm-cm
0.00000431 ohm-cm