| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | Chi Mei Corporation (ChiMei) |
| Trade Name | Wonderloy® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Chi Mei Wonderloy® PC-365 PC/ABS Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 46.0 MPa | 6670 psi | 50 mm/min; ISO 527 |
| Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
| Elongation at Break | 80 % | 80 % | 50 mm/min; ISO 527 |
| Flexural Strength | 80.0 MPa | 11600 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | ISO 180/4A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 106 °C | 223 °F | annealed; ISO 75 |
| 117 °C | 243 °F | unannealed; ISO 75 | |
| Vicat Softening Point | 123 °C @Load 5.00 kg |
253 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| 136 °C @Load 1.00 kg |
277 °F @Load 2.20 lb |
50°C/hr; ISO 306 | |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0590 in |