Material Notes:
FeaturesChevron Rykon Premium Grease No. 1364 contains polyurea thickener in highly refined paraffinic oil, as well as extreme pressure and rust protection additives. Chevron Rykon Premium Grease No. 1364:is resistant to oil separation during use and storage. has excellent high temperature characteristics.will not blacken copper or steel when tested for one hour at 150°C (302°F).ApplicationsChevron Rykon Premium Grease No. 1364 was formulated specifically for the automotive constant velocity (CV) driveline joints used in front-wheel drive automobiles.It is compatible with the common elastomers used for boots in the joints and can be used in "hot" CV joints up to 177°C (350°F).Chevron Rykon Premium Grease No. 1364 can also be used in other applications requiring a high temperature grease with extreme pressure additives.Chevron Rykon Premium Grease No. 1364 meets the requirements of GKN specification M-3005 for CV grease.
Physical Properties Metric English Comments
Viscosity Measurement 90
90
Viscosity Inex of base oil; ASTM D2270
Saybolt Viscosity at 100°F 596 SUS
596 SUS
Saybolt Viscosity at 210°F 76 SUS
76 SUS
Kinematic Viscosity at 40°C (104°F) 115 cSt
115 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 14.1 cSt
14.1 cSt
ASTM D445
Mechanical Properties Metric English Comments
Penetration 312
312
Worked
Timken Test 18100 g
40.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Dropping Point 243 °C
469 °F
Descriptive Properties Value Comments
Bearing Rust Pass
Color Blue
Texture Smooth
Thickener, % / type 10 / Polyurea