Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco NLGI 2 Ultra Duty Grease EP

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco NLGI 2 Ultra Duty Grease EP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They are manufactured using selected highly refined, high viscosity base oils, a lithuium-12 hydroxystearate thickener, rust and oxidation inhibitors, and extreme pressure and tackiness additives. They are red in color and stringy in texture.Chevron Ultra-Duty Greases EP provide thicker shock absorbing oil film protection and greater water resistance than conventional multipurpose greases due to their high viscosity components.The high viscosity components and tackiness additive give Chevron Ultra-Duty Greases EP an excellent adhesive quality which provides a tenacious lubricating film in working parts. The lubricants stay in place under severe abrasive operating conditions to resist water washout and shock load wear.The outstanding tackiness characteristics of Chevron Ultra-Duty Greases EP make these products somewhat harder to pump than the historical soft, buttery greases. For this reason, we recommend the use of a heavy follower play with air driven grease pumps.Chevron Ultra-Duty Greases EP lubricate well at low temperatures. The ASTM D 1478 low temperature torque test shows that they retain their lubricating capacity, as defined by military specification MIL-G-81322, sown to about -26°C (-15°F).ApplicationsChevron Ultra-Duty Greases EP are recommended for use in automotive and industrial equipment operating under severe service except were very high operating temperatures are encountered. Typical application are: mining equipment, construction equipment, material handling equipment, marine deck equipment, amine deck cranes, oil filed equipment, offshore drilling equipment, paper machines, dredging equipment, logging equipment, rock quarry equipment, etc., operating in water, mud, or dusty conditions.Chevron Ultra-Duty Greases EP will provide the needed shock load and rust protection and, best of all, they stay put which means less frequent regreasing. They are not our primary recommendation for high temperature wheel bearings. Chevron Delo® Greases EP, Chevron RPM® Automotive LC Greases EP, or Chevron Black Pearl® Greases EP are preferred for wheel bearing applicationsIn industrial service, Chevron Ultra-Duty Greases EP are recommended for use in all types of plain and antifriction bearings from 1-1/2 inch OD to over 16 inch OD, operating at speeds from 50 to 3000 rpm, as well as slides, gears, ways, etc.
Physical Properties Metric English Comments
Viscosity Measurement 76
76
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 2160 SUS
2160 SUS
Saybolt Viscosity at 210°F 121 SUS
121 SUS
Kinematic Viscosity at 40°C (104°F) 400 cSt
400 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 24.3 cSt
24.3 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Weld Point
Penetration 280
280
Worked
Penetration P(0), 1/10 mm 275
275
Timken Test 31700 g
70.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 143 °C
289 °F
Minimum Service Temperature, Air -5.00 °C
23.0 °F
Flash Point 274 °C
525 °F
ASTM D92
Dropping Point 190 °C
374 °F
Descriptive Properties Value Comments
Color Red
Lincoln Ventmeter, psig at 30 s, at 0°F 2500
Lincoln Ventmeter, psig at 30 s, at 30°F 600
Lincoln Ventmeter, psig at 30 s, at 75°F 280
Texture Stringy
Thickener, % / type 8.6 / Lithium
Copyright © lookpolymers.com All Rights Reserved