ChevronTexaco GST® EP ISO 46 Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name GST®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco GST® EP ISO 46 Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent recommendation for many other industrial applications including air compression. Chevron GST Oils are formulated with ISOSYN® base stocks.Higher temperatures in advanced gas and steam turbines require a circulating system oil with exceptional high temperature stability. Chevron GST Oils have outstanding thermal and oxidation stability.Nonvolatile oxidation inhibition minimizes the evaporative loss of the inhibitors, a common problem with turbine oils where bearing temperatures are high and system capacities are limited. With retained oxidation resistance for long periods under high temperature conditions, Chevron GST Oils have proven they will provide longer oil service life and reduced turbine down time.Corrosion inhibition protects costly turbine shafts and gears from corrosion and rusting. Chevron GST Oils have excellent demulsibility characteristics which allow these oils to maintain a high film strength coating on critical wear points of bearings and gear reducers and assure fast removal of water contamination.Foam inhibition prevents sump overflow and erratic governor operation.ApplicationsChevron GST Oils are recommended for use in turbines of all types including gas, steam, and hydroelectric turbines, and marine gear turbine sets.
Physical Properties Metric English Comments
API Gravity 32 °
32 °
Viscosity Measurement 101
101
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 225 SUS
225 SUS
Saybolt Viscosity at 210°F 48.2 SUS
48.2 SUS
Kinematic Viscosity at 40°C (104°F) 43.7 cSt
43.7 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 6.6 cSt
6.6 cSt
ASTM D445
Oxidative Stability 21.67 hour
21.67 hour
25 psi pressure drop; ASTM D2272
10000 hour
10000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
Thermal Properties Metric English Comments
Pour Point -36.0 °C
-32.8 °F
ASTM D97
Flash Point 224 °C
435 °F
ASTM D92
Descriptive Properties Value Comments
FZG, Pass stage, DIN 51354 12