Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Delo® 3000 Marine Engine Oil, SAE 40

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Delo®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ChevronTexaco Delo® 3000 Marine Engine Oil, SAE 40.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesChevron Marine Engine Oil Delo 3000 Marine is a high quality engine oils developed for use in a wide variety of medium speed trunk piston engines burning residual fuels.It is manufactured using high quality base oils and dispersant, detergent, antioxidant, antiwear, and alkaline reserve additives.The base number or alkalinity of this oil is 30. The detergent/dispersant properties of this oil provides exceptionally clean crankcases and keep oil control rings clean. These properties reduce lube oil filter blockage and provide excellent insolubles control handling characteristics.Chevron Marine Engine Oil 3000 Marine has extremely good viscosity control in severe high temperature service.It has a high degree of water tolerance. Water can be centrifuged out with essentially no loss of additive. Water washing of the oil, however, is not recommended.ApplicationsChevron Marine Engine Oil Delo 3000 Marine is recommended for use in medium speed trunk piston engines burning residual fuels with up to 3.5% sulfur content.The antiwear additives contained in Chevron Marine Engine Oil Delo 3000 Marine provide outstanding load carrying and antiwear characteristics. In the FZG (A/8, 3/90) gear test, the fail stage for Chevron Marine Engine Oil Delo 3000 Marine was Stage 10. The FZG values permit this oil to be used in engine reduction gears and other applications where additional EP/ antiwear properties are required.Chevron Marine Engine Oil Delo 3000 Marine meets the requirements of API Service Category CF. It is approved by all major engine manufacturers for use in their medium speed engines.
Physical Properties Metric English Comments
API Gravity 23.8 °
23.8 °
Viscosity Measurement 100
100
Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 143 cSt
143 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
ASTM D445
Ash 3.95 %
3.95 %
Sulfated Ash wt%
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
ASTM D97
Flash Point 250 °C
482 °F
ASTM D92
Component Elements Properties Metric English Comments
Phosphorous, P 0.046 %
0.046 %
Zinc, Zn 0.056 %
0.056 %
Chemical Properties Metric English Comments
Total Base Number 30
30
ASTM D2896
Users viewing this material also viewed the following: