Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Compound H Rust Proof

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Compound H Rust Proof.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Texaco Rust Proof Compounds deliver value through:Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the elements. Good water displacing capabilities ensures that the protective film is also waterproof. The special rust inhibitor system ensures maximum protection against corrosive attack. Good penetrating characteristics ensure difficult-to-reach seams and crevices receive effective corrosion protection.Minimum surface preparation required — Ability to penetrate existing flaky or heavy rust means that little or no preliminary cleaning of metal surfaces is required before application. This penetrating ability makes existing rust easier to remove, should it be considered desirable to do so for a better or more economical job.Minimal cost — Self-sealing properties of the protective film minimizes the need for touch-ups when film damage occurs through scratches or brush marks. The overall cost of this soft film rust protection is much less than ordinary paint.Easy removal — Soft protective film is readily soluble in petroleum solvent or kerosine to enable easy removal when required.Texaco Rust Proof Compounds are soft film rust preventives designed for relatively long-term protection of iron and steel.They are formulated from high melting point petrolatums and a special rust inhibitor system with penetrating and water displacing capabilities.Texaco Rust Proof Compounds are recommended for:Iron and steel exposed to atmospheric conditions before, during and after manufacturing into finished partsUndercoating of vehiclesTransformer casingsBridges and floating bridge pontoonsNonfood storage vesselsNonpotable water tanksBallast tanksGas holdersHoisting equipmentFarm implementsMay be applied by brush, dip or spray.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221977; MSDS Number: 9038
Physical Properties Metric English Comments
Ash <= 0.10 %
<= 0.10 %
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 142
142
25°C (77°F), Undisturbed
Thermal Properties Metric English Comments
Melting Point 69.0 °C
156 °F
Minimum Service Temperature, Air 27.0 °C
80.6 °F
Brush
54.0 - 66.0 °C
129 - 151 °F
Spray
66.0 - 79.0 °C
151 - 174 °F
Dip
Flash Point 243 °C
469 °F
Descriptive Properties Value Comments
Solvent, max, wt% 0.1