Material Notes:
HSD11 is a general, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness and machinability, and good heat seal strength and dimensional stability. One side has corona treatment with a normal sealing temperature. It is widely used in food and confectionary packaging, packing, printing, and laminating applications.Information provided by Kinlead.
Physical Properties Metric English Comments
Thickness 30.0 microns
1.18 mil
± 2.5%; ASTM-252-78
Linear Mold Shrinkage 0.030 cm/cm
0.030 in/in
ASTM-D1204
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM-D1204
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 185 %
185 %
ASTM-D882
Film Elongation at Break, TD 65 %
65 %
ASTM-D882
Coefficient of Friction 0.30
0.30
T/T-US; ASTM-D1894
0.30
0.30
T/O-US; ASTM-D1894
Film Tensile Strength at Break, MD 140 MPa
20300 psi
ASTM-D882
Film Tensile Strength at Break, TD 280 MPa
40600 psi
ASTM-D882
Heat Seal Strength 517.9 g/25 mm
1.142 lb/in
Kinlead
Heat Seal Strength Initiation Temperature 115 - 120 °C
239 - 248 °F
Kinlead
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM-D1003
Gloss 92 %
92 %
ASTM-D1003
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Corona Treatment (Dyn) 38
ASTM-D2578
Wetting Tension (Dyn) 38
ASTM-D2578
Yield (m²/kg) 36.6