Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 69.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Melting Point 69.0 °C
156 °F
Freezing Point, DSC; ASTM D3418
DuPont Bynel® 39E622 Adhesive Resin  (discontinued **)
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 69.0 °C
156 °F
Exxon Method
ExxonMobil Escorene® UL-7750 EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
Melting Point 69.0 °C
156 °F
ASTM D3418
SK Chemicals SKYTHANE® 310 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Melting Point 69.0 - 72.0 °C
156 - 162 °F
Suqian Unitechem Efficient Inhibitor 701
Chemical Name: 4-Hydroxy-2,2,6,6-tetramethyl-piperidinooxy (TMHPO')CAS NO.: 2226-96-2Molecular Formula: C9H18NO2Uses: It can prevent alkene from self-polymerization, or control and adjust the degree..
Melting Point 69.0 °C
156 °F
ASTM D3418
SK Chemicals SKYTHANE® UB310 Co-Extruding Adhesive
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Melting Point 69.0 °C
156 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 3101 Acid-/Acrylate-Modified EVA Adhesive Resin
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Melting Point 69.0 - 98.0 °C
156 - 208 °F
ASTM D3418(DSC)
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Melting Point 69.0 °C
156 °F
ChevronTexaco Compound H Rust Proof
Texaco Rust Proof Compounds deliver value through:Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the..
Melting Point 69.0 °C
156 °F
DSC
Arkema Group LOTRYL® Bestpeel 2407 Copolymer Ethylene - Methyl Acrylate
LOTRYL® Bestpeel 2407 is a ready-to-use thermoplastic composition designed to make peelable heat seal layers onto various substrates. The base resin is a random copolymer of ethylene and methyl acr..
Copyright © lookpolymers.com All Rights Reserved