Material Notes:
Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceHigh coefficient of friction Applications: Typical cast film applications include: Personal careGeneral purposeInformation provided by Phillips
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D-1505
Water Vapor Transmission 13.0 g/m²/day
0.837 g/100 in²/day
Blown Film at 1.25 mil; ASTM F-1249
Oxygen Transmission Rate 6100 cc/m²/day
393 cc/100 in²/day
Blown Film at 1.25 mil; ASTM D-3985
Melt Index of Compound 4.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Antiblock Level 0.00 ppm
0.00 ppm
Slip Level 0.00 ppm
0.00 ppm
Mechanical Properties Metric English Comments
Coefficient of Friction 0.75
0.75
Blown Film at 1.25 mil; ASTM D-1894
Elmendorf Tear Strength, MD 12.6 g/micron
320 g/mil
Blown Film at 1.25 mil; ASTM D-1922
Elmendorf Tear Strength, TD 4.92 g/micron
125 g/mil
Blown Film at 1.25 mil; ASTM D-1922
Dart Drop 2.56 g/micron
65.0 g/mil
Blown Film at 1.25 mil; ASTM D-1709
Thermal Properties Metric English Comments
Melting Point 109 °C
228 °F
ASTM D-3418
Vicat Softening Point 99.0 °C
210 °F
ASTM D-1525
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
Blown Film at 1.25 mil; ASTM D-1003
Gloss 86 %
86 %
60°, Blown Film at 1.25 mil; ASTM D-2457