Chesterton 783 ACR Anti-Seize Compound

Category Fluid , Lubricant
Manufacturer Chesterton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 783 ACR Anti-Seize Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chesterton® 783 ACR represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants, 783 ACR can be used under extremely severe conditions of temperature and pressure to assist in assembly and disassembly of threaded components. 783 ACR can be used over a broad temperature range. Hardening will not occur when used between -34°C to 900°C (-30°F to 1650°F).Features:No Toxic Heavy MetalsFor Extreme Pressure= up to 8928 kg/cm2 (126,983 psi)Broad Service Temperature RangeUltra-Fine ParticlesCorrosion ResistantWaterproofBenefits:Safer to workersUsable under most extreme conditionsFills in microscopic voidsSuggested Uses: Bolts, screws, studs, pipe threads, press fits, pump sleeves and splines. Use in power plants, textiles mills, bakeries, foundries, steel mills, boiler rooms, oil refineries, marine applications, chemical plants, automotive industry.Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
Particle Size <= 11 µm
<= 11 µm
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 168.7
168.7
ASTM D2596, DIN 51 350
127000
127000
[psi]; ASTM D2596, DIN 51 350
Four Ball Extreme Pressure, Weld Load 800 kg
1760 lb (mass)
ASTM D2596, DIN 51 350
Penetration 270
270
ASTM D217, ISO2137
K Factor (Wear Factor) 0.14
0.14
Skidmore - Wilhelm Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 900 °C
1650 °F
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Dropping Point >= 288 °C
>= 550 °F
ASTM D566, ISO2176
Descriptive Properties Value Comments
Color Light gray
Consistency 2
NLGI
Soft Paste
Copper Corrosion 2A
24 hrs. @ 100°C (212°F), ASTM D4048, DIN 51 811
Corrosion Resistance >1200 hrs.
@ 100 microns, 5% NaCl, ASTM B117
Water Washout Resistance <0.13%
@ 79°C, ASTM D1264