Chengdu Polyster 9502 High Performance Grade TPV

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster 9502 High Performance Grade TPV.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd.
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
GB 2411
Tensile Strength, Ultimate 14.6 MPa
2120 psi
GB/T 528
Elongation at Break 400 %
400 %
GB/T 528
Tear Strength 65.0 kN/m
371 pli
GB/T 529
Compression Set 40 %

@Temperature 23.0 °C
40 %

@Temperature 73.4 °F
GB/T 7759
60 %

@Temperature 100 °C
60 %

@Temperature 212 °F
GB/T 7759
Tensile Set 45 %
45 %
100%; GB/T 528
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
GB 5470