3M Cold Seal® 3130 Polyethylene Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Cold Seal®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Cold Seal® 3130 Polyethylene Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Cold Seal® Polyethylene Tape 3130 is a temporary tape with a self-sealing latex emulsion and feature a self-adhering cohesive coating which bonds to itself and not to the product to be packaged and the result is an airtight pouch that is resistant to moisture, dirt and grease.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.70 MPa
247 psi
ASTM D3759
Elongation at Break 450 %
450 %
ASTM D3759
Peel Strength 0.153 kN/m
0.875 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Natural rubber latex emulsion