Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster 6502 High Performance Grade TPV

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Chengdu Polyster Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster 6502 High Performance Grade TPV.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd.
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
GB 2411
Tensile Strength, Ultimate 6.30 MPa
914 psi
GB/T 528
Elongation at Break 450 %
450 %
GB/T 528
Tear Strength 46.0 kN/m
262 pli
GB/T 529
Compression Set 23 %

@Temperature 23.0 °C
23 %

@Temperature 73.4 °F
GB/T 7759
35 %

@Temperature 100 °C
35 %

@Temperature 212 °F
GB/T 7759
Tensile Set 10 %
10 %
100%; GB/T 528
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
GB 5470
Users viewing this material also viewed the following: