Chengdu Polyster 6500 General Grade TPV

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster 6500 General Grade TPV.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chengdu Polyster Co., Ltd.
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
GB 2411
Tensile Strength, Ultimate 7.50 MPa
1090 psi
GB/T 528
Elongation at Break 450 %
450 %
GB/T 528
Tear Strength 40.0 kN/m
228 pli
GB/T 529
Compression Set 29 %

@Temperature 23.0 °C
29 %

@Temperature 73.4 °F
GB/T 7759
40 %

@Temperature 100 °C
40 %

@Temperature 212 °F
GB/T 7759
Tensile Set 18 %
18 %
100%; GB/T 528
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
GB 5470