Polykemi AB SCANTEC PC S60R GF30 Polycarbonate, Glass-Fiber Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled
Manufacturer Polykemi AB
Trade Name SCANTEC
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Polykemi AB SCANTEC PC S60R GF30 Polycarbonate, Glass-Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Filler Content 30 %
30 %
±2%; Polykemi
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
With Flow; ISO 2577
0.0040 cm/cm
0.0040 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 100 MPa
<= 14500 psi
ISO/R527
Elongation at Break 2.0 %
2.0 %
ISO/R527
Flexural Strength <= 165 MPa
<= 23900 psi
ISO 178
Flexural Modulus 7.00 GPa

@Temperature 23.0 °C
1020 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
120°C/h; ISO 75/1
Vicat Softening Point 147 °C

@Load 5.001 kg
297 °F

@Load 11.03 lb
50°C/h; ISO 306
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-1

@Thickness 3.20 mm
V-1

@Thickness 0.126 in
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
IEC 695-2-1