Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

California Fine Wire Nickel 211 (Nickel Manganese Alloy)

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Nickel 211 (Nickel Manganese Alloy).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.72 g/cc
0.315 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 517 MPa
75000 psi
Annealed
793 MPa
115000 psi
Stress relieved
965 MPa
140000 psi
Hard
Thermal Properties Metric English Comments
Thermal Conductivity 49.3 W/m-K
342 BTU-in/hr-ft²-°F
Melting Point 1430 °C
2610 °F
Maximum Service Temperature, Air 500 °C
932 °F
Operating Temperature
Component Elements Properties Metric English Comments
Manganese, Mn 4.75 %
4.75 %
Nickel, Ni 93.7 %
93.7 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000170 ohm-cm
0.0000170 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.0032 ohms/ohm-°C
0-100°C