Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CRP Technology Windform® FX Polyamide Composite

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Nylon
Manufacturer CRP Technology
Trade Name Windform®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CRP Technology Windform® FX Polyamide Composite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive Manufacturing applications. White colored, Windform® FX is characterized by exceptional resistance and resilience to repeated bending and torsion applications; excellent impact resistance; consistency and behaviour similar to polypropylene and ABS injection moulded parts. Windform® FX is perfect for building accurate, reliable and long lasting prototypes; no further treatments are needed. The powder also benefits from extended recycling and lower refresh rates.Sample applications: Flexible components, functional parts with living hinges or clip fittings. In addition, ducts of a complex shape, with thin walls, particularly suited for aerospace and motorsport, dashboards and grids, fenders, fans and connectors.Information provided by CRP Technology.
Physical Properties Metric English Comments
Density 1.027 g/cc
0.03710 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.96 MPa
7101 psi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Elongation at Break 43.9 %
43.9 %
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Tensile Modulus 1.357 GPa
196.8 ksi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Flexural Strength 45.0 MPa
6530 psi
UNI EN ISO 14125: 2000
Flexural Modulus 0.952 GPa
138 ksi
UNI EN ISO 14125: 2000
Charpy Impact Unnotched 3.172 J/cm²
15.10 ft-lb/in²
ISO 179-1:2007
Charpy Impact, Notched 0.325 J/cm²
1.55 ft-lb/in²
ISO 179-1:2007
Thermal Properties Metric English Comments
Melting Point 190.7 °C
375.3 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 47.10 °C
116.8 °F
ASTM D648
Vicat Softening Point 187.6 °C
369.7 °F
10 N; ASTM D1525
Electrical Properties Metric English Comments
Electrical Resistivity 2.30e+14 ohm-cm
2.30e+14 ohm-cm
ASTM D257
Surface Resistance 9.00e+13 ohm
9.00e+13 ohm
ASTM D257
Descriptive Properties Value Comments
Color White
Surface Finish 2.0 Ra µm
After Finishing
6.0 Ra µm
After SLS Process