Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® ELKONIUM 33 platinum based alloy

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer CMW Inc.
Trade Name ELKONIUM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONIUM 33 platinum based alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (1769(C) and good resistance to forming arcs. Low electrical conductivity (15% IACS) limits its application to low currents, usually below 5 amperes. Because of the high cost of the platinum ELKONIUM alloys, they are almost always supplied as composite contacts with thin facings of the ELKONIUM metal (silver brazed to nickel plated steel backings in the form of rivets, screws and weld buttons).ELKONIUM 33 and ELKONIUM 331 material grades have higher ruthenium content and have essentially the same hardness as the platinum-iridium alloy, ELKONIUM 32. It is less expensive than CMW's ELKONIUM 32 material. Because of its high hardness, it is used in many magneto applications. All five alloys have low transfer characteristics and are used in voltage regulators and motor speed governors. They can be used as a positive contact paired with tungsten negative contact for improved transfer resistance. They also have high tarnish resistance and are suitable for many sensitive, low voltage applications.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 19.9 g/cc
0.719 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 91
91
annealed
96
96
cold worked
Tensile Strength, Ultimate 586 MPa
85000 psi
annealed
1030 MPa
150000 psi
cold worked
Elongation at Break 4.0 %
4.0 %
cold worked
12 %
12 %
annealed
Component Elements Properties Metric English Comments
Platinum, Pt 89 %
89 %
Ruthenium, Ru 11 %
11 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000430 ohm-cm
0.0000430 ohm-cm
4 % IACS