Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CIMBAR RP 9305 Talc

Category Ceramic , Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR RP 9305 Talc.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. RP 9300 Series talcs are platy, hydrophobic and non-abrasive.9300 Series talcs industrial applications include: thermoplastics, thermosets, adhesives & mastics.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 2.78 g/cc
2.78 g/cc
Bulk Density 0.368 g/cc
0.0133 lb/in³
Loose
0.961 g/cc
0.0347 lb/in³
Tapped
Brightness 91 %
91 %
Hunter Rd, dry
Oil Absorption 26 %
26 %
g oil/100 g filler; ASTM D281
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Loss On Ignition 17 %
17 %
Particle Size 1.2 µm
1.2 µm
@ 10%; Micrometrics Sedigraph 5100
5.5 µm
5.5 µm
Median
27 µm
27 µm
@ 98%; Micrometrics Sedigraph 5100
Particle Mesh Size 325 Mesh
325 Mesh
0.1% retained
pH 9.0
9.0
Component Elements Properties Metric English Comments
Al2O3 <= 1.0 %
<= 1.0 %
CaO <= 13 %
<= 13 %
Fe2O3 <= 1.0 %
<= 1.0 %
MgO 24 %
24 %
SiO2 46 %
46 %