Braskem TI4005F Impact copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TI4005F Impact copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Extra high izod impact, very high flexural modulus, good low temperature drop impact.Applications: Suggested uses include compounding and thermoforming.Process: Thermoforming.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM D785
Tensile Strength 29.0 MPa
4200 psi
2 in/min; ASTM D638
Elongation at Yield 10.5 %
10.5 %
2 in/min; ASTM D638
Flexural Modulus 1.34 GPa
195 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched NB
NB
ASTM D256A
Impact Test 48.8 J

@Temperature -29.0 °C
36.0 ft-lb

@Temperature -20.2 °F
ASTM D3763