Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Absolan® 2300 Sparkle SAN

Category Polymer , Thermoplastic , SAN Polymer
Manufacturer Styrolution
Trade Name Absolan®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Styrolution Absolan® 2300 Sparkle SAN.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Absolac 2300 Sparkle is a good flow gradeInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Melt Flow >= 45 g/10 min

@Load 10.0 kg,
Temperature 220 °C
>= 45 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 690 MPa
100000 psi
ISO 527
Thermal Properties Metric English Comments
Vicat Softening Point 103 °C

@Load 5.10 kg
217 °F

@Load 11.2 lb
120°C/h; ASTM D 1525