Braskem F1000HC Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem F1000HC Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive, AppliancesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDAInformation provided by Braskem
Physical Properties Metric English Comments
Melt Flow 115 g/10 min

@Load 2.16 kg,
Temperature 230 °C
115 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 41.0 MPa
5950 psi
2 in/min; ASTM D638
Elongation at Yield 4.5 %
4.5 %
2 in/min; ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256A