Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem Evateno® 8019 PE EVA Foam Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Braskem
Trade Name Evateno®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Braskem Evateno® 8019 PE EVA Foam Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Evateno® 8019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium Vinyl-Acetate content. Evateno® 8019 PE is an easy processing and crosslinkable product with high compatibility with other thermoplastic and elastomeric resins, and inorganic fillers. It offers high elasticity, high environmental stress cracking resistance (ESCR), impact strength and low temperatures resistance.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM-D1505 / ASTM-D792
ESCR 100% Igepal® >= 300 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
>= 300 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Vinyl Acetate Content 19 %
19 %
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM-D2240
Hardness, Shore D 30
30
ASTM-D2240
Thermal Properties Metric English Comments
Melting Point 86.0 °C
187 °F
ASTM-D3418
Vicat Softening Point 58.0 °C

@Load 1.02 kg
136 °F

@Load 2.25 lb
ASTM-D1525