Material Notes:
CA8200 is a low-density polyethylene for extrusion coating. CA8200 contains no additives. Applications: extrusion coating of high volume production of boards and papers, and coating of various plastic films and cellophane.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Neck In 6.80 cm
2.68 in
BTM 14920
Coating Weight >= 7.50 g/m²
>= 4.69 lb/ream
BTM 14922
Descriptive Properties Value Comments
Coating Speed (m/min) < 850
BTM 14921