Blue River Coatings Conversion Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Blue River Coatings
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Blue River Coatings Conversion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BLUE RIVER COATINGS CONVERSION COATING is a water-based product that eliminates rust by accomplishing two functions at the same time. First, rust is converted to ferric iron, a black organic compound. Second, a coating of clear acrylic is formed over the coated area. The surface that remains after the transformation can be either left black or coated with Blue River Coatings wide range of products for the desired outcome. Product tests have shown that Blue River Conversion Coating has extended the life of equipment or products for several more years after probable replacement. Blue River Coatings Conversion Coating can be used on all rusted surfaces. Enviromental Advantages:BLUE RIVER COATINGS CONVERSION COATING is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with your local and state regulations for proper handling. Characteristics:Excellent durabilityCan be applied to interior and exterior surfacesFinal coating can be paintedDistilled water is used for reductionWater is used for clean-upNon-HazardousCoating will not flash rust on bare metalShelf life of 1 yearUnused product can be returned to containerNon-Flammable UsesSchools Industrial PlantsHomesFarmsMachineryAutomobilesHeavy EquipmentBoatsToolsRailroadsInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Volatile Organic Compounds (VOC) Content 35 g/l
35 g/l
Thermal Properties Metric English Comments
Boiling Point 100 °C
212 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Dust Free, at 50% humidity
60.0 min

@Temperature 75.0 °C
1.00 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Evaporation Rate Slower than ether
Flexibility Good
Pencil Hardness HB
Salt Spray Good
Solvent Resistance Good
Vapor Density Heavier than air