BLUE RIVER COATINGS CRC100-H is a two-component inorganic corrosion resistant coating designed for Original Equipment Manufacturers (OEM) to protect metal substrates from corrosion and abrasion. If gouged or damaged, the coating will not experience creepage and is repairable. The product is designed to coat surfaces that require a hard, abrasive, and chemical resistant coating that can withstand temperatures of 1,800°F. CRC100-H offers excellent durability and corrosion protection as well as being a low VOC and EPA compliant coating. Enviromental Advantages:BLUE RIVER COATINGS CRC100-H is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be dried and sent to a “Class B” landfill. Please follow local and state regulations in the proper use and disposal of this product. Characteristics:Excellent hardnessExcellent adhesion to oxidized metalExcellent hardnessExcellent heat tolerance (1800°F+)Excellent acid resistanceGood impact resistance and flexibility Available in flat finish onlyNon-photochemically reactiveApplication by spraying or dippingSolvent is used for clean-upAir dry Product life of 48 hours UsesSteelAluminumInformation provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Density 1.21 g/cc
0.0437 lb/in³
Solids Content 47.5 %
47.5 %
by volume
48 %
48 %
by weight
Volatile Organic Compounds (VOC) Content 246 g/l
246 g/l
Mechanical Properties Metric English Comments
Impact Test 18.1 J
13.3 ft-lb
Forward and Reverse
Thermal Properties Metric English Comments
Flash Point 8.33 °C
47.0 °F
Part A
65.6 °C
150 °F
Part B
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 75.0 °C
4.00 hour

@Temperature 167 °F
Recoat, at 50% humidity
720 min

@Temperature 75.0 °C
12.0 hour

@Temperature 167 °F
Dust Free, at 50% humidity
Descriptive Properties Value Comments
Evaporation Rate Slower than ether
Flexibility 1/8" conical mandrel
Pencil Hardness 4H
Salt Spray Pass
Non-oxidized steel panel, 2,000 hours with no blistering, creepage, cracking, peeling, or delamination.
Pass;
Oxidized steel panel, 1000 hours no blistering, creepage, cracking, peeling or delamination.
Solvent Resistance 20; double rubs with lacquer thinner, acetone, MEK, and xylene with saturated cloth
Submersion Test >5 years
liquid fertilizer (nitrogen) with no blistering, cracking, peeling or delamination.
30 minutes
30 minutes in Hydrochloric Acid (10%) with no blistering cracking peeling or delamination.
30 minutes
Sulfuric Acid (10%) with no blistering, cracking, peeling or delamination.
Theoretical Coverage 762 ft2 at 1 mil