Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bisalloy Steels BisPlate 80PV Thickness 16-80 mm

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel , Carbon Steel , Low Carbon Steel , Pressure Vessel Steel
Manufacturer Bisalloy Steels
Trade Name BisPlate
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bisalloy Steels BisPlate 80PV Thickness 16-80 mm.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage Tanks, Railroad Tankers, Refinery and Petro Chemical EquipmentTesting: AS/NZS 3597 Grade 700PV NATA approvedWelding: According to AS/NZS 1554 parts 4 and 5Tolerance: In accordance with AS/NZS 1365
Mechanical Properties Metric English Comments
Hardness, Brinell 255
255
Tensile Strength at Break 830 MPa
120000 psi
Tensile Strength, Yield 750 MPa

@Strain 0.200 %
109000 psi

@Strain 0.200 %
Elongation at Break 26 %
26 %
in 50 mm GL
Charpy Impact 55.0 J

@Temperature -20.0 °C
40.6 ft-lb

@Temperature -4.00 °F
Transverse
Component Elements Properties Metric English Comments
Boron, B 0.0010 %
0.0010 %
Carbon, C 0.18 %
0.18 %
Chromium, Cr 0.20 %
0.20 %
Iron, Fe 97.8 %
97.8 %
As Balance
Manganese, Mn 1.4 %
1.4 %
Molybdenum, Mo 0.20 %
0.20 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0030 %
0.0030 %
Descriptive Properties Value Comments
CE (IIW) 0.5
PCM 0.29
Surface Finish Shotblasted