Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bisalloy Steels BisPlate 60 Thickness 5 -

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel , Carbon Steel , Low Carbon Steel
Manufacturer Bisalloy Steels
Trade Name BisPlate
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bisalloy Steels BisPlate 60 Thickness 5 -.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness.Applications: Storage Tanks, High Rise Buildings, Lifting EquipmentTesting: AS/NZS 3597 Grade 500 NATA approvedWelding: According to AS/NZS 1554 parts 4 and 5Tolerance: In accordance with AS/NZS 1365
Mechanical Properties Metric English Comments
Hardness, Brinell 210
210
Tensile Strength at Break 640 MPa
92800 psi
Tensile Strength, Yield 580 MPa

@Strain 0.200 %
84100 psi

@Strain 0.200 %
Elongation at Break 30 %
30 %
in 50 mm GL
Charpy Impact 200 J

@Temperature -20.0 °C
148 ft-lb

@Temperature -4.00 °F
Longitudinal
Component Elements Properties Metric English Comments
Boron, B 0.0010 %
0.0010 %
Carbon, C 0.16 %
0.16 %
Iron, Fe 98.3 %
98.3 %
As Balance
Manganese, Mn 1.1 %
1.1 %
Molybdenum, Mo 0.20 %
0.20 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0030 %
0.0030 %
Descriptive Properties Value Comments
CE (IIW) 0.4
PCM 0.25
Surface Finish Shotblasted
Users viewing this material also viewed the following: