Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TPE-VInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength at Break 3.50 MPa
508 psi
ISO 527-1
Elongation at Break 500 %
500 %
ISO 527-1
Descriptive Properties Value Comments
Resin Type TPE-V
Users viewing this material also viewed the following: