Unifrax Fiberfrax® Topcoat™ 2600 Insulating Mix

Category Ceramic
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® Topcoat™ 2600 Insulating Mix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiberfrax Pumpable-LDS, Pumpable-GS, and Topcoat 2600 Insulating Mix were designed for application into difficult-to-reach areas requiring insulation. Fiberfrax Pumpable-LDS and Pumpable-GS have temperature grade ratings of 1260°C (2300°F). Fiberfrax Topcoat 2600 Insulating Mix has a temperature grade rating of 1426°C (2600°F). A conventional air-operated extrusion pump permits application of these products directly from their container into furnace and boiler hot spots, refractory cracks, furnace door jambs, and other areas requiring high-temperature insulating and sealing.Typical ApplicationsHot face repairs of ceramic fiber liningsSacrificial lining for areas of mechanical abuseRefractory lining veneerInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.561 g/cc
0.0203 lb/in³
Dry
1.28 g/cc
0.0463 lb/in³
Wet
Solids Content 45 %
45 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000965 GPa
0.140 ksi
Dry
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1343 °C
2449 °F
Recommended Operating Temperature
Shrinkage 1.2 %

@Temperature 1340 °C,
Time 86400 sec
1.2 %

@Temperature 2440 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Appearance Brown putty
Molten Aluminum Wetting Resistance Fair
Temperature Grade (°F) 2600