Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Pluracol® 1168 Rigid Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 1168 Rigid Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Pluracol® 1168 Polyol is a general purpose aromatic initiator-based polyol for rigid foams for use in a variety of applications. It is attractively priced for consideration for foaming insulated panels, refrigerators, trailers, furniture, etc., by pour-in-place or frothing techniques. Foams made with Pluracol 1168 Polyol are characterized by fine cell structure, low K factor, and good dimensional stability. Pluracol 1168 Polyol is not recommended for use in quasi-prepolymer preparation.Information provided by BASF
Physical Properties Metric English Comments
Density 1.059 g/cc

@Temperature 45.0 °C
0.03826 lb/in³

@Temperature 113 °F
1.063 g/cc

@Temperature 35.0 °C
0.03840 lb/in³

@Temperature 95.0 °F
1.067 g/cc

@Temperature 25.0 °C
0.03855 lb/in³

@Temperature 77.0 °F
Viscosity 357 cP

@Temperature 45.0 °C
357 cP

@Temperature 113 °F
758 cP

@Temperature 35.0 °C
758 cP

@Temperature 95.0 °F
1880 cP

@Temperature 25.0 °C
1880 cP

@Temperature 77.0 °F
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
STI 3062
Descriptive Properties Value Comments
Color Amber Liquid
Hydroxyl Number 285 - 315 mg KOH/g
STI 3007/3162
Users viewing this material also viewed the following: