BASF Elastollan® S98A Polyester Type Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer BASF
Trade Name Elastollan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan® S98A Polyester Type Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
ASTM D2240
Hardness, Shore D 54
54
ASTM D2240
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D412
Tensile Strength, Yield 19.0 MPa

@Strain 100 %
2760 psi

@Strain 100 %
ASTM D-412
32.0 MPa

@Strain 300 %
4640 psi

@Strain 300 %
ASTM D-412
Elongation at Break 425 %
425 %
ASTM D412
Tear Strength 180 kN/m
1030 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 70
70
H-18 wheel; ASTM D-1044.
Tensile Set 80 %
80 %
at break; ASTM D-412