BASF Elastollan 1154 D KFFC TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer BASF
Trade Name Elastollan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan 1154 D KFFC TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilience performance. Typical Applications: Polyether based for flexible flat cables.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ISO 686
Tensile Strength 16.5 MPa
2390 psi
20; ISO 37
22.0 MPa
3190 psi
100; ISO 37
31.5 MPa
4570 psi
300; ISO 37
40.0 MPa
5800 psi
ISO 37
Elongation at Break 400 %
400 %
ISO 37
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
DIN ISO 179
9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
DIN ISO 179
Tear Strength 150 kN/m
856 pli
DIN ISO 34-1/Bb
Abrasion 30
30
[mm<sup>3</sup>; ISO 4649
Compression Set 30 %

@Temperature 23.0 °C
30 %

@Temperature 73.4 °F
DIN EN ISO 815
45 %

@Temperature 70.0 °C
45 %

@Temperature 158 °F
DIN EN ISO 815
Processing Properties Metric English Comments
Processing Temperature 175 - 220 °C
347 - 428 °F
Extrusion
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Extrusion