BASF AMIX TI

Category Fluid
Manufacturer BASF
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF AMIX TI.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Formula: C9H21NO3CAS: 122-20-3Description: AMIX TI is a dark solid that is almost odorless. It is fully soluble in waterSynonyms: TRIPA, 1,1’,1”-Nitrilotri-2-propanol, Tri-2-propanolamine, Tri-iso-propanolamine, Tris(2-propanol)amine, Tris(2-Hydroxypropyl)amineApplications: Used as a chemical intermediateInformation provided by BASF
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Thermal Properties Metric English Comments
Melting Point 39.0 °C
102 °F
Boiling Point 240 - 370 °C
464 - 698 °F
Flash Point 155 °C
311 °F
Processing Properties Metric English Comments
Moisture Content 1.0 %
1.0 %
DIN 51 777
Descriptive Properties Value Comments
Composition Triisopropanolamine
>97%
Ignition Temperature 295°C