Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 10752 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Axiall 10752 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose 75C jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.37 - 1.41 g/cc
1.37 - 1.41 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78
72 - 78
delayed; ASTM D-2240
Tensile Strength, Yield 14.1 MPa
2050 psi
ASTM D-638
Elongation at Yield 304.9 %
304.9 %
Air Aging: 240 hours @ 100°C; 30 mil slabs; UL 1581
350 %
350 %
ASTM D-638
100% Modulus 0.00655 GPa
0.950 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D-746
Oxygen Index 25.5 %
25.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 171 °C
340 °F
Users viewing this material also viewed the following: