Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon T1020-R004-## 0.020" Self-Fusing Silicone Rubber Tape

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon T1020-R004-## 0.020" Self-Fusing Silicone Rubber Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
1 inch wide, 20 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number.Design/Construction:Interleave: 1 mil PolyesterRubber: Self-fusing Silicone RubberCross-section: 1" wide rectangularThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Water Absorption 0.10 %
0.10 %
Arlon SQA-TMS-016
Thickness 508 microns
20.0 mil
Rubber; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
Silicone Property; ASTM D2240
Tensile Strength 9.846 MPa
1428 psi
Silicone Property; ASTM D412
Elongation at Break 699 %
699 %
Silicone Property; ASTM D412
Peel Strength 0.596 kN/m
3.40 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 260 °C
500 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 32.8 kV/mm
834 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red