Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Silicone Hose and Duct Material with Polyester Substrate (65390R042)  (discontinued **)

Category Polymer , Thermoset , Silicone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Silicone Hose and Duct Material with Polyester Substrate (65390R042)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Side one - uncured silicone, 0.005 in., -0.001(0.1 mm, -0.01); Substrate - 6500 Polyester Fabric, 0.038 in. (0.97 mm) nominal; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.042 in +0.004,-0.001 (1.1 mm + 0.1,-0.03). Color: Red. Weight: 1695 g/m² ± 136 (50.0 oz./yd.² ± 4). Shelf Life: 6 months from date of manufacture at 21°C (70°F). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Peel strength is 62 kPa (9.0 psi).Applications: Hose and duct material.Information provided by the manufacturer, Arlon Silicone Technologies Division.
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Tensile Strength, Ultimate 4.18 - 5.42 MPa
606 - 786 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.6 °C
-69.9 °F
Electrical Properties Metric English Comments
Dielectric Strength 14.76 - 23.62 kV/mm
374.9 - 599.9 kV/in