Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 30850S085 0.085" Uncured, Unsupported Silicone Rubber on Release Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 30850S085 0.085" Uncured, Unsupported Silicone Rubber on Release Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Substrate
2160 microns
85.0 mil
Rubber
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Silicone Property
Tensile Strength >= 6.89 MPa
>= 1000 psi
Silicone Property
Elongation at Break >= 700 %
>= 700 %
Silicone Property
Tear Strength >= 35.1 kN/m
>= 200 pli
Silicone Property
Compression Set <= 28 %
<= 28 %
Silicone Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 177 °C
0.500 hour

@Temperature 350 °F
Recommended Cure Cycle
240 min

@Temperature 227 °C
4.00 hour

@Temperature 440 °F
Recommended Post Cure Cycle
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
Descriptive Properties Value Comments
Color Saddle Brown
Total Product Weight (oz/yd2) 71.5