Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group OREVAC® 18350 Grafted Maleic Anhydride Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group OREVAC® 18350 Grafted Maleic Anhydride Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
OREVAC 18350 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion performances between an epoxy primer and LACQTENE 2006PBK35 from Total Petrochemicals. It combined with MDPE or HDPE and a epoxy to fulfill the requirement of different application standards such as NFA 49-710 or DIN 30670 when applied in the rules of art. OREVAC 18350 is recommended for pipeline service temperature up to 80°C.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.931 g/cc
0.0336 lb/in³
ISO 1183
Melt Index of Compound 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ISO 608
Tensile Strength, Yield 12.4 MPa
1800 psi
ISO R 527-2
Elongation at Break >= 600 %
>= 600 %
ISO R 527-2
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
DSC
Maximum Service Temperature, Air <= 80.0 °C
<= 176 °F
Vicat Softening Point 107 °C

@Load 0.999 kg
225 °F

@Load 2.20 lb
ISO 306
Users viewing this material also viewed the following: