Arkema Group Evatane® 1080 VN 5 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer Arkema
Trade Name Evatane®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Evatane® 1080 VN 5 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets, medical.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Melt Flow 10.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.00 MPa
435 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.0500 GPa
7.25 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 86.0 °C
187 °F
10°C/min
Vicat Softening Point 61.0 °C
142 °F
50°C/hr; 50N
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.