ArcelorMittal TRIP 780 Very high strength steel, Cold Rolled Steel

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer ArcelorMittal
Trade Name TRIP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ArcelorMittal TRIP 780 Very high strength steel, Cold Rolled Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Available in the following: uncoated (HCT780T), electrogalvanized (HCT780T+ZE) and Extragal®/Galvannealed (HCT780T+Z/+ZZF)Description: TRIP steels offer an outstanding combination of strength and ductility as a result of their microstructure. They are thus suitable for structural and reinforcement parts of complex shape. The microstructure of these steels is composed of islands of hard residual austenite and carbide-free bainite dispersed in a soft ferritic matrix. Austenite is transformed into martensite during plastic deformation (TRIP: TRansformation Induced Plasticity effect), making it possible to achieve greater elongations and lending these steels their excellent combination of strength and ductility. These steels have high strain hardening capacity. They exhibit good strain redistribution and thus good drawability. As a result of strain hardening, the mechanical properties, and especially the yield strength, of the finished part are far superior to those of the initial blank. High strain hardening capacity and high mechanical strength lend these steels excellent energy absorption capacity. TRIP steels also exhibit a strong bake hardening (BH) effect following deformation, which further improves their crash performance. The TRIP range of steels comprises 2 cold rolled grades in both uncoated and coated formats (TRIP 690 and TRIP 780) and one hot rolled grade (TRIP 780), identified by their minimum tensile strength expressed in MPa.Applications: As a result of their high energy absorption capacity and fatigue strength, TRIP steels are particularly well suited for automotive structural and safety parts such as cross members, longitudinal beams, B-pillar reinforcements, sills and bumper reinforcements. ArcelorMittal has extensive data on the forming and service characteristics of the TRIP family of steels. To integrate these steels at the design stage, a team of experts is available to carry out specific studies based on modeling and experimental tests.Information provided by ArcelorMittal
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 780 - 900 MPa
113000 - 131000 psi
Tensile Strength, Yield 460 - 550 MPa
66700 - 79800 psi
Elongation at Break >= 23 %
>= 23 %
L<Sub>0</sub>=80 mm, th<3 mm
Component Elements Properties Metric English Comments
Carbon, C <= 0.25 %
<= 0.25 %
Iron, Fe >= 95.75 %
>= 95.75 %
as balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Silicon, Si <= 2.0 %
<= 2.0 %