Category | Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) |
Manufacturer | AlphaGary |
Trade Name | AlphaSeal™ |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary AlphaSeal™ 240-6CY Blue 7002 Polyolefin Thermoplastic Elastomer.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.930 g/cc | 0.930 g/cc |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 93 | 93 | |
Tensile Strength | 11.7 MPa | 1700 psi | |
Elongation at Break | 550 % | 550 % |