Physical Properties Metric English Comments
Density 6.90 - 7.30 g/cc
0.249 - 0.264 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 300 - 500
300 - 500
Tensile Strength, Ultimate 80.0 - 300 MPa
11600 - 43500 psi
Modulus of Elasticity 100 - 200 GPa
14500 - 29000 ksi
Compressive Strength 300 - 400 MPa
43500 - 58000 psi
Thermal Properties Metric English Comments
CTE, linear 10.0 - 13.0 µm/m-°C

@Temperature 20.0 °C
5.56 - 7.22 µin/in-°F

@Temperature 68.0 °F
Parallel DOM
Specific Heat Capacity 0.350 - 0.500 J/g-°C
0.0837 - 0.120 BTU/lb-°F
Thermal Conductivity 10.0 - 200 W/m-K
69.4 - 1390 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 450 °C
842 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000400 - 0.0000700 ohm-cm
0.0000400 - 0.0000700 ohm-cm
Magnetic Coercive Force, Hc 700 Oe
700 Oe
710 Oe
710 Oe
Intrinsic
Magnetic Remanence, Br 10000 Gauss
10000 Gauss
Magnetic Maximum Energy Product, BH 3.0 MGOe
3.0 MGOe
Curie Temperature 850 °C
1560 °F
Descriptive Properties Value Comments
Reversible Temp Coef., Bd -0.02 %/°C
Temperature Coefficient, Br -0.025 %/°C
(20-100°C)
Temperature Coefficient, Hci +0.01 %/°C
(20-100°C)