Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Alcoa 2324-T39 Aluminum Plate

Category Metal , Nonferrous Metal , Aluminum Alloy , 2000 Series Aluminum Alloy
Manufacturer Alcoa
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Alcoa 2324-T39 Aluminum Plate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy 2324-T39 is a higher strength version of alloy 2024-T351 and is a purity controlled composition variant of alloy 2024. It was developed for tension-dominated, fatigue and fracture critical plate applications. The T39 temper, developed through special fabricating practices, improves both strength and fracture toughness properties over alloy 2024 plate. Alloy 2324-T39 plate is being used successfully on lower wing skin and center wing box components of commercial aircraft.Information provided by Alcoa.
Physical Properties Metric English Comments
Density 2.77 g/cc
0.100 lb/in³
per Aluminum Association
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 475 MPa
>= 68900 psi
Guaranteed minimum; long transverse
Tensile Strength, Yield >= 370 MPa
>= 53700 psi
Guaranteed minimum; long transverse
Elongation at Break >= 8.0 %
>= 8.0 %
Guaranteed minimum; long transverse
Modulus of Elasticity 72.4 GPa
10500 ksi
AA2024
Poissons Ratio 0.33
0.33
AA2024
Shear Modulus 27.0 GPa
3920 ksi
AA2024
Thermal Properties Metric English Comments
CTE, linear 23.2 µm/m-°C

@Temperature 20.0 °C
12.9 µin/in-°F

@Temperature 68.0 °F
AA2024
24.7 µm/m-°C

@Temperature 20.0 - 300 °C
13.7 µin/in-°F

@Temperature 68.0 - 572 °F
average; AA2024
Specific Heat Capacity 0.875 J/g-°C
0.209 BTU/lb-°F
AA2024
Thermal Conductivity 151 W/m-K
1050 BTU-in/hr-ft²-°F
AA2024
Component Elements Properties Metric English Comments
Aluminum, Al 92 - 94.7 %
92 - 94.7 %
As Remainder
Chromium, Cr <= 0.10 %
<= 0.10 %
Copper, Cu 3.8 - 4.4 %
3.8 - 4.4 %
Iron, Fe <= 0.12 %
<= 0.12 %
Magnesium, Mg 1.2 - 1.8 %
1.2 - 1.8 %
Manganese, Mn 0.30 - 0.90 %
0.30 - 0.90 %
Other, each <= 0.050 %
<= 0.050 %
Other, total <= 0.15 %
<= 0.15 %
Silicon, Si <= 0.10 %
<= 0.10 %
Titanium, Ti <= 0.15 %
<= 0.15 %
Zinc, Zn <= 0.25 %
<= 0.25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000449 ohm-cm
0.00000449 ohm-cm
AA2024
Users viewing this material also viewed the following: