Akzo Nobel Expancel® 461 DE 20 d70 Dry expanded microspheres

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Akzo Nobel, Expancel
Trade Name Expancel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Expancel® 461 DE 20 d70 Dry expanded microspheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the thermoplastic shell softens and the gas increases its pressure, resulting in an expansion of the spheres.Applications: Car underbody coatings; Auto body filler and marine and hobby putties; Cable fillings; Cultured marble; Civil explosives; Modelmaking materials; Sealants (acrylics, PUR, polysulphides, silicones); Synthetic wood
Physical Properties Metric English Comments
Density 0.0640 - 0.0760 g/cc
0.00231 - 0.00275 lb/in³
Particle Size 15 - 25 µm
15 - 25 µm
D(0.5)
Descriptive Properties Value Comments
Solvent Resistance 4
Scale of 1 to 5